Rame Berillio 2
Chemical Composition % Description
Be 1,8 2,1
Co 0,3
Ni 0,3
Fe 0,2
Cu resto
Alloy undergoes heat treatment and it is therefore recommended that the recrystallization temparature NOT be exceeded during the metalworking process.
Products Applications
• drawn square, round and flat bars
• Slabs
• Plates and discs
• Support blocks for projection welding
•Plastic moulds
• Highly stressed machine parts with significant heat dispersion
Mechanical properties Standards and Benchmarks
Hardness HBW 2,5/187,5 350-420
Electrical conductivity.. IACS% 15-20
Ultimate strength N/mm2 970-1200
Recrystallization temparature 300°-320°
Extension A% 5-7
Yield point N/mm2 490-550
ISO CuBe2
ALTEC RBT 400
CEN CW101C
UNI-EN 12165
Copyright Altec s.r.l. - P.IVA 01748440128 - All right reserverd 2015 - Best view 1024x768 - Mail: info@altecrame.it - Cookie policy