Be
|
0,4-0,7
|
Material is
provided with
Certificate of Compliance
|
Co
|
1,5-2,8
|
Ni
|
0,4
|
Fe
|
0,2
|
Cu
|
resto
|
|
By forging dripped
and lathe cut ingots, we are able to extract metal products weighing between 10
and 300 kg inclusive. This type of alloy undergoes a particular heat treatment providing
superior hardness. It is therefore recommended that the recrystallization temparature
NOT be exceeded during the metalworking process in order to ensure that mechanical
properties are not compromised.
|